Injection molding cycle

From Plastics Wiki, free encyclopedia

Jump to: navigation, search

The basic injection cycle is as follows: Mold close - injection carriage forward - inject plastic -metering - carriage retract - mold open - eject part(s)

For the injection molding cycle to begin, four criteria must be met: mold open, ejector pins retracted, shot built, and carriage forward. When these criteria are met, the cycle begins with the mold closing. This is typically done as fast as possible with a slow down near the end of travel.

Contents

Mold close

The molds are closed shut by hydraulics or electric, and the heated plastic is forced by the pressure of the injection screw to take the shape of the mold. Some machines are run by electric motors instead of hydraulics or a combination of both. The water-cooling channels then assist in cooling the mold and the heated plastic solidifies into the part. Improper cooling can result in distorted molding or one that is burnt.

Mold safety is low speed and low pressure mold closing. It usually begins just before the leader pins of the mold and must be set properly to prevent accidental mold damage. When the mold halves touch clamp tonnage is built.

Inject plastic

Next, molten plastic material is injected into the mold. The material travels into the mold via the sprue bushing, then the runner system delivers the material to the gate. The gate directs the material into the mold cavity to form the desired part. This injection usually occurs under velocity control. When the part is nearly full, injection control is switched from velocity control to pressure control. This is referred to as the pack/hold phase of the cycle. Pressure must be maintained on the material until the gate solidifies to prevent material from flowing back out of the cavity. Cooling time is dependent primarily on the wall thickness of the part. During the cooling portion of the cycle after the gate has solidified, plastication takes place. Plastication is the process of melting material and preparing the next shot. The material begins in the hopper and enters the barrel through the feed throat. The feed throat must be cooled to prevent plastic pellets from fusing together from the barrel heat. The barrel contains a screw that primarily uses shear to melt the pellets and consists of three sections. The first section is the feed section which conveys the pellets forward and allows barrel heat to soften the pellets. The flight depth is uniform and deepest in this section. The next section is the transition section and is responsible for melting the material through shear. The flight depth continuously decreases in this section, compressing the material. The final section is the metering section which features a shallow flight depth, improves the melt quality and color dispersion. At the front of the screw is the non-return valve which allows the screw to act as both an extruder and a plunger. When the screw is moving backwards to build a shot, the non-return assembly allows material to flow in front of the screw creating a melt pool or shot. During injection, the non-return assembly prevents the shot from flowing back into the screw sections.

Mold open

Once the shot has been built and the cooling time has timed out, the mold opens. Mold opening must occur slow-fast-slow. The mold must be opened slowly to release the vacuum that is caused by the injection molding process and prevent the part from staying on the stationary mold half. This is undesirable because the ejection system is on the moving mold half. Then the mold is opened as far as needed, if robots are not being used, the mold only has to open far enough for the part to be removed. A slowdown near the end of travel must be utilized to compensate for the momentum of the mold. Without slowing down the machine cannot maintain accurate positions and may slam to a stop damaging the machine. Once the mold is open, the ejector pins are moved forward, ejecting the part.

Shot built

The resin, or raw material for injection molding, is usually in pellet or granule form, and is melted by heat and shearing forces shortly before being injected into the mold. Resin pellets are poured into the feed hopper, a large open bottomed container, which feeds the granules down to the screw. The screw is rotated by a motor, feeding pellets up the screw's grooves. The depth of the screw flights decreases towards the end of the screw nearest the mold, compressing the heated plastic. As the screw rotates, the pellets are moved forward in the screw and they undergo extreme pressure and friction which generates most of the heat needed to melt the pellets. Heaters on either side of the screw assist in the heating and temperature control during the melting process.

Eject part(s)

The cycle is completed when the mold opens and the part is ejected with the assistance of ejector pins within the mold. When the ejector pins retract, all criteria for a molding cycle have been met and the next cycle can begin.

The channels through which the plastic flows toward the chamber will also solidify, forming an attached frame. This frame is composed of the sprue, which is the main channel from the reservoir of molten resin, parallel with the direction of draw, and runners, which are perpendicular to the direction of draw, and are used to convey molten resin to the gate(s), or point(s) of injection. The sprue and runner system can be cut or twisted off and recycled, sometimes being granulated next to the mold machine. Some molds are designed so that the part is automatically stripped through action of the mold.